Test Method Color |
N/A Visual |
Color |
N/A Beige |
Test metod Carrier |
N/A Visual |
Reinforcement Carrier |
N/A Kapton ® MT |
Test Method Thicknesses |
N/A ASTM D374 |
Thickness |
N/A 0.08 mm0.003 in |
Thickness Tolerance |
N/A ± 0.013 mm± 0.0005 in |
Test Method Specific Gravity |
N/A ASTM D792 |
Specific Gravity |
N/A 1.70 |
Test Method Hardness |
N/A ASTM D2240 |
Hardness, Shore A |
N/A 90 |
Operating Temperature Range |
N/A –40 to 200 ºC–40 to 392 ºF |
Test Method Thermal Impedance |
N/A ASTM D5470 |
Thermal Impedance |
N/A 2.4 ºC-cm²/W0.37 ºC-in²/W |
Test Method Apparen Thermal Conductivity |
N/A ASTM D5470 |
Apparen Thermal Conductivity |
N/A 0.4 W/m·K |
Test Method Heat Capacity |
N/A ASTM E1269 |
Heat Capacity |
N/A 1.0 J/g-ºC |
Test Method Coefficient of Thermal Expansion |
N/A ASTM E831 |
Coefficient of Thermal Expansion |
N/A 400 ppm/ºC |
Test Method Volume Resistivity Dry |
N/A ASTM D257 |
Volume Resistivity Dry |
N/A 1014 O/cm |
Test Method Volume Resistivity Wet |
N/A ASTM D257 |
Volume Resistivity Wet |
N/A Not tested |
Test Method Voltage Breakdown Dry |
N/A ASTM D149 |
Voltage Breakdown Dry |
N/A 5000 Vac |
Test Method Voltage Breakdown Wet |
N/A ASTM D149 |
Voltage Breakdown Wet |
N/A Not tested |
Test Method Tensile Strength |
N/A ASTM D412 |
Tensile Strength |
N/A 20.7 MPa3000 psi |
Test Method Tear Strength |
N/A ASTM D642 |
Tear Strength |
N/A 26.3 kN/m150 lb/in |
Test Method Elongation |
N/A ASTM D412 |
Test Method Flammability Rating |
N/A UL 94 |
Flammability Rating |
N/A V-0 |
Test Method RoHS Compliant |
N/A Chomeric Certification |
RoHS Compliant |
N/A Yes |
Test Method Outgassing |
N/A ASTM E595 |
Outgassing TML |
N/A Not tested |
Outgassing CVCM |
N/A Not tested |
Test Method Shelf Life |
N/A Chomerics |
Shelf Life, Months from Dry Pad |
N/A 12 |
Shelf Life, Months from Dry Pad with PSA |
N/A 12 |