COHRlastic solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durometer to the relatively hard 70 durometer on the Shore A scale. It is manufactured in different formulations to provide a choice of physical properties and cost considerations.

Series 300-700 COHRlastic generalpurpose molded sheet is available in thicknesses up to 1/2" and it withstands temperatures from –100 °F to +500more
Unit of Measure
Items
Silicone Solid Rubber

Silicone Solid Rubber Tape

Silicone Solid Rubber

Silicone Solid Rubber Tape

Silicone Solid Rubber

Silicone Solid Rubber Tape

Silicone Solid Rubber

Silicone Solid Rubber Tape

Silicone Solid Rubber

Silicone Solid Rubber Tape
Dielectric Strength Approx. N/A 500 V/mil
Thermal Conductivity (Average) N/A 4.4 x 10-4 x (cal·cm/ºC·cm·s) 1.3 BTU i./h·ft2 ºF
Specific Heat N/A 0.3 BTU/lb/ºF
Linear Thermal Expansion1 N/A 1.5 x 10-4
Width/Sheet Size N/A 36 x 36 in
Color N/A Red
Thickness2 N/A 1/2 ±.031 in1/4 ±.031 in N/A 1/16 ±.016 in1/2 ±.016 in1/4 ±.016 in1/8 ±.016 in3/16 ±.016 in3/32 ±.016 in3/8 ±.016 in5/16 ±.016 in N/A 1/16 ±.016 in1/2 ±.016 in1/4 ±.016 in1/8 ±.016 in3/16 ±.016 in3/32 ±.016 in3/8 ±.016 in5/16 ±.016 in N/A 1/16 ±.016 in1/2 ±.016 in1/4 ±.016 in1/8 ±.016 in3/16 ±.016 in3/32 ±.016 in3/8 ±.016 in5/16 ±.016 in N/A 1/16 ±.016 in1/2 ±.016 in1/4 ±.016 in1/8 ±.016 in3/16 ±.016 in3/32 ±.016 in3/8 ±.016 in5/16 ±.016 in
ZZ-R-765, Class 2a & 2b (Grade) N/A N/A 40 N/A 50 N/A 60 N/A 70
ZZ-R-765, Class 3b (Grade) N/A
AMS N/A N/A 3301 N/A 3302 N/A 3303 N/A 3304
Test Method Durometer N/A D2240
Durometer (Shore A ±5)3 N/A 30 N/A 40 N/A 50 N/A 60 N/A 70
Test Method Tensile Strength N/A D412
Tensile Strength4 N/A 800 psi N/A 700 psi N/A 700 psi N/A 700 psi N/A 700 psi
Test Method Elongation N/A D412
Elongation5 N/A 550 % N/A 400 % N/A 350 % N/A 200 % N/A 160 %
Test Method Tear Strength N/A D624
Tear Strength6 N/A 50 ppi N/A 75 ppi N/A 70 ppi N/A 65 ppi N/A 60 ppi
Test Method Compression Set N/A D395
Compression Set after 70 h at 320 ºF7 N/A 15 %
Durometer Change (Points, Shore A) after Dry Heat Aging for 70 h at 437 ºF N/A +5
Tensile Strength Change after Dry Heat Aging for 70 h at 437 ºF N/A –15 %
Elongation Change after Dry Heat Aging for 70 h at 437 ºF N/A –15 %
Durometer Change (Points, Shore A) after Immersion in ASTM Oil #1 (High Aniline Point) for 70 H at 302 ºF N/A –5 N/A –5 N/A –5 N/A –5 N/A –10
Tensile Strength Change after Immersion in ASTM Oil #1 (High Aniline Point) for 70 H at 302 ºF N/A –10 %
Elongation Change after Immersion in ASTM Oil #1 (High Aniline Point) for 70 H at 302 ºF N/A –10 %
Volume Change after Immersion in ASTM Oil #1 (High Aniline Point) for 70 H at 302 ºF N/A +10 % N/A +5 % N/A +5 % N/A +5 % N/A +5 %
  • 1 Room temperature to +350 ºF
  • 2 Thickness 3/32 in - special order. Minimum quantities apply.
  • 3 Die B Method B, ASTM D2000 + Fed. Spec. ZZ-R-765.
  • 4 Die B Method B, ASTM D2000 + Fed. Spec. ZZ-R-765.
  • 5 Die B Method B, ASTM D2000 + Fed. Spec. ZZ-R-765.
  • 6 Die B Method B, ASTM D2000 + Fed. Spec. ZZ-R-765.
  • 7 Die B Method B, ASTM D2000 + Fed. Spec. ZZ-R-765.