Test Method Color
|
|
Visual
|
|
Color
|
|
Beige
|
|
Test metod Carrier
|
|
Visual
|
|
Reinforcement Carrier
|
|
Kapton ® MT
|
|
Test Method Thicknesses
|
|
ASTM D374
|
|
Thickness
|
|
0.08 mm 0.003 in
|
|
Thickness Tolerance
|
|
± 0.013 mm ± 0.0005 in
|
|
Test Method Specific Gravity
|
|
ASTM D792
|
|
Specific Gravity
|
|
1.70
|
|
Test Method Hardness
|
|
ASTM D2240
|
|
Hardness, Shore A
|
|
90
|
|
Operating Temperature Range
|
|
–40 to 200 ºC –40 to 392 ºF
|
|
Test Method Thermal Impedance
|
|
ASTM D5470
|
|
Thermal Impedance
|
|
2.4 ºC-cm²/W 0.37 ºC-in²/W
|
|
Test Method Apparen Thermal Conductivity
|
|
ASTM D5470
|
|
Apparen Thermal Conductivity
|
|
0.4 W/m·K
|
|
Test Method Heat Capacity
|
|
ASTM E1269
|
|
Heat Capacity
|
|
1.0 J/g-ºC
|
|
Test Method Coefficient of Thermal Expansion
|
|
ASTM E831
|
|
Coefficient of Thermal Expansion
|
|
400 ppm/ºC
|
|
Test Method Volume Resistivity Dry
|
|
ASTM D257
|
|
Volume Resistivity Dry
|
|
1014 O/cm
|
|
Test Method Volume Resistivity Wet
|
|
ASTM D257
|
|
Volume Resistivity Wet
|
|
Not tested
|
|
Test Method Voltage Breakdown Dry
|
|
ASTM D149
|
|
Voltage Breakdown Dry
|
|
5000 Vac
|
|
Test Method Voltage Breakdown Wet
|
|
ASTM D149
|
|
Voltage Breakdown Wet
|
|
Not tested
|
|
Test Method Tensile Strength
|
|
ASTM D412
|
|
Tensile Strength
|
|
20.7 MPa 3000 psi
|
|
Test Method Tear Strength
|
|
ASTM D642
|
|
Tear Strength
|
|
26.3 kN/m 150 lb/in
|
|
Test Method Elongation
|
|
ASTM D412
|
|
Test Method Flammability Rating
|
|
UL 94
|
|
Flammability Rating
|
|
V-0
|
|
Test Method RoHS Compliant
|
|
Chomeric Certification
|
|
RoHS Compliant
|
|
Yes
|
|
Test Method Outgassing
|
|
ASTM E595
|
|
Outgassing TML
|
|
Not tested
|
|
Outgassing CVCM
|
|
Not tested
|
|
Test Method Shelf Life
|
|
Chomerics
|
|
Shelf Life, Months from Dry Pad
|
|
12
|
|
Shelf Life, Months from Dry Pad with PSA
|
|
12
|
|