| Items |
CCH-36-101-0050 CHO-FOIL Conductive Tapes |
CCH-36-101-0100 CHO-FOIL Conductive Tapes |
CCH-36-101-0150 CHO-FOIL Conductive Tapes |
CCH-36-101-0200 CHO-FOIL Conductive Tapes |
CCH-36-101-0300 CHO-FOIL Conductive Tapes |
|||||
| Tape Description | N/A Copper foil, conductive adhesive version | |||||||||
| Tape Width | N/A 0.5 in12.7 mm | N/A 1.0 in25.4 mm | N/A 1.5 in38.1 mm | N/A 2.0 in50.8 mm | N/A 3.0 in76.2 mm | |||||
| Part Number Prefix | N/A CCH | |||||||||
| Foil/Fabric Type | N/A 1 oz. RA Copper | |||||||||
| Foil/Fabric Thickness | N/A 1.4 mil0.0356 mm | |||||||||
| Adhesive Type | N/A Electrically Conductive, Pressure-Sensitive Acrylic | |||||||||
| Adhesive Thickness | N/A 1.5 mil0.0381 mm | |||||||||
| Total Thickness1 | N/A 2.9 mil0.0737 mm | |||||||||
| Temperature Range | N/A –40 to 400 ºF–40 to 205 ºC | |||||||||
| Test Method Flame Resistance | N/A UL Subject 510 | |||||||||
| Flame Resistance | N/A Pass | |||||||||
| Test Method Adhesion to Aluminum | N/A ASTM D1000 | |||||||||
| Adhesion to Aluminum | N/A > 40 oz/in2.5 ppi438 N/m | |||||||||
| Test Method Electrical Resistance | N/A MIL-STD-202C | |||||||||
| Electrical Resistance | N/A < 0.003 O/in²< 0.0005 O/cm² | |||||||||
| Test Method Initial Surface Resistivity | N/A CHO-TP-57 | |||||||||
| Initial Surface Resistivity2 | N/A < 2 mO | |||||||||
| Test Method Initial Through Resistivity | N/A CHO-TP-57 | |||||||||
| Initial Through Resistivity3 | N/A < 3 mO | |||||||||
| Test Method Initial Peel Strength | N/A ASTM D1000 | |||||||||
| Initial Peel Strength4 | N/A 44.8 oz/in2.8 ppi490 N/m | |||||||||
| Test Method Initial Taber Abrasion Surface Resistivity | N/A CHO-TP-57 | |||||||||
| Initial Taber Abrasion Surface Resistivity | N/A < 6 mO | |||||||||
| Test Method Heat Aging 185 ºF (85 ºC)/168 h, Surface Resistivity | N/A CHO-TP-57 | |||||||||
| Heat Aging 185 ºF (85 ºC)/168 h, Surface Resistivity | N/A < 10 mO | |||||||||
| Test Method Heat Aging 185 ºF (85 ºC)/168 h, Through Resistivity | N/A CHO-TP-57 | |||||||||
| Heat Aging 185 ºF (85 ºC)/168 h, Through Resistivity5 | N/A <16 mO | |||||||||
| Test Method Heat Aging 185 ºF (85 ºC)/168 h, Peel | N/A ASTM D1000 | |||||||||
| Heat Aging 185 ºF (85 ºC)/168 h, Peel | N/A 57.6 oz/in3.6 ppi630 N/m | |||||||||
| Test Method Heat Aging 250 ºF (121 ºC)/168 h, Surface Resistivity | N/A CHO-TP-57 | |||||||||
| Heat Aging 250 ºF (121 ºC)/168 h, Surface Resistivity | N/A <10 mO | |||||||||
| Test Method Heat Aging 250 ºF (121 ºC)/168 h, Through Resistivity | N/A CHO-TP-57 | |||||||||
| Heat Aging 250 ºF (121 ºC)/168 h, Through Resistivity | N/A < 70 mO | |||||||||
| Test Method Heat Aging 250 ºF (121 ºC)/168 h, Peel | N/A ASTM D1000 | |||||||||
| Heat Aging 250 ºF (121 ºC)/168 h, Peel | N/A 57.6 oz/in3.6 ppi630 N/m | |||||||||
| Test Method Heat Aging with Humidity 95 % RH/ 185 ºF (85 ºC)/168 h, Surface Resistivity | N/A CHO-TP-57 | |||||||||
| Heat Aging with Humidity 95 % RH/ 185 ºF (85 ºC)/168 h, Surface Resistivity | N/A | |||||||||
| Test Method Heat Aging with Humidity 95 % RH/ 185 ºF (85 ºC)/168 h, Through Resistivity | N/A CHO-TP-57 | |||||||||
| Heat Aging with Humidity 95 % RH/ 185 ºF (85 ºC)/168 h, Through Resistivity | N/A | |||||||||
| Test Method Heat Aging with Humidity 95 % RH/ 185 ºF (85 ºC)/168 h, Peel | N/A ASTM D1000 | |||||||||
| Heat Aging with Humidity 95 % RH/ 185 ºF (85 ºC)/168 h, Peel | N/A | |||||||||
| Test Method Salt Fog Corrosion/168 h, Surface Resistivity | N/A CHO-TP-57 | |||||||||
| Salt Fog Corrosion/168 h, Surface Resistivity | N/A | |||||||||
| Test Method Salt Fog Corrosion/168 h, Through Resistivity | N/A CHO-TP-57 | |||||||||
| Salt Fog Corrosion/168 h, Through Resistivity | N/A | |||||||||
| Test Method Salt Fog Corrosion/168 h, Peel | N/A ASTM D1000 | |||||||||
| Salt Fog Corrosion/168 h, Peel | N/A | |||||||||
| Test Method Taber Abrasion 500 g Weight, CS-10 Wheel, 500 Cycles | N/A CHO-TP-57 | |||||||||
| Taber Abrasion 500 g Weight, CS-10 Wheel, 500 Cycles | N/A < 3 mO | |||||||||
|
||||||||||